Skip to main content

Table 3 Ratios of PSS to PEDOT from the area under XPS graphs

From: Preparation, morphology and thermoelectric performance of PEDOT/CuI nanocomposites

Sample

PEDOT area

PSS area

PSS to PEDOT

Pristine PEDOT: PSS

0.05437

0.12111

2.2275

DMSO-PEDOT: PSS

0.06286

0.13038

2.0741

PEDOT/CuI (1.9 vol%)

0.00597

0.1272

1.8847

PEDOT/CuI (4.8 vol%)

0.06412

0.1186

1.8493

PEDOT/CuI (6.9 vol%)

0.0654

0.1173

1.7934

PEDOT/CuI (9.2 vol%)

0.0642

0.1147

1.7975