From: Heat treated graphene thin films for reduced void content of interlaminar enhanced CF/PEEK composites

Fig. 5

Compressive shear strength of CF/PEEK Control samples and 1 wt% percent loading added to the interlaminar regions with and without heat treatment. All samples are within the range of an autoclave manufactured sample (25.70 ± 3.76 MPa) [54]. Error bars denote one standard deviation of the mean. The inset image depicts the interlaminar shear plane induced by the loading noses