From: Effect of tungsten disulfide nanotubes on crystallization of polylactide under uniaxial deformation and annealing
WS2 concentration
(wt%)
Xc (%)
UNST
ST0
ST3
ST10
0
9.0
19
32.1
38.0
0.1
9.8
15.4
42.4
41.6
0.2
10.9
22.7
42.7
41.4
0.3
9.6
21.8
41.1
42.1
0.6
9.1
39.1
39.9