Fig. 5From: Thermoplastic elastomer composite strips with damage detection capabilities for self-healing elastomersa Stress–strain curve and b relative resistance curve during the tensile test up to the point fracture for the printed composite sensor elements based on the two TPS matrix materials with a Shore hardness 40A and 50A, before and after the thermal treatment at 105 °C for 30 minBack to article page